Advertisements
Advertisements
Question
The electrolyte used in Hall and Heroult process is:
Options
Alumina (20%)
Cryolite (60%)
Fluorspar (20%)
All of these
MCQ
Advertisements
Solution
All of these
Explanation:
The electrolytic bath used in this extraction process is a fused mixture consisting of roughly 20% alumina, 60% cryolite, and 20% fluorspar.