Electrolytic cell for the extraction of aluminium:

shaalaa.com
  क्या इस प्रश्न या उत्तर में कोई त्रुटि है?
2012-2013 (October)

वीडियो ट्यूटोरियलVIEW ALL [1]

संबंधित प्रश्न

Write the names and chemical formulae of any one ore of iron.


Write the reactions involved in the zone of reduction in blast furnace during extraction of iron.


Out of C and CO, which is a better reducing agent at the lower temperature range in the blast furnace to extract iron from the oxide ore?


Fe2O3 is reduced to spongy iron near the top of blast furance by

(A) H2

(B) CaO

(C) SiO2

(D) CO


Mention names and formulae of two ores of alumunium.


Draw neat and labelled diagram of Bessermer converter used in the extraction of copper.


What is the role of cryolite in the extraction of aluminium?


In the extraction of Al, impure Al2O3 is dissolved in conc. NaOH to form sodium aluminate and leaving impurities behind. What is the name of this process?


What is the role of coke in the extraction of iron from its oxides?


Differentiate between “minerals” and “ores”.


Write the names and chemical formulae of any ‘two’ minerals of aluminium.


What is 'copper matte' ?


A current liberates 0.50 g of hydrogen in 2 hours. The weight of copper (at. wt. = 63.5) deposited at the same time by the same current through copper sulphate solution is ______.


What happens when a nickel rod is dipped into a copper sulphate solution? Justify your answer.

[\[\ce{E{^{\circ}_{Ni^{+2}/Ni}}}\] = − 0.25 V and \[\ce{E{^{\circ}_{Cu^{+2}/Cu}}}\] = +0.34 V]


Bauxite has the composition


Give the uses of zinc.


Which of the following options are correct?

(i) Cast iron is obtained by remelting pig iron with scrap iron and coke using hot air blast.

(ii) In extraction of silver, silver is extracted as cationic complex.

(iii) Nickel is purified by zone refining.

(iv) Zr and Ti are purified by van Arkel method.


In the extraction of aluminium by Hall-Heroult process, purified \[\ce{Al2O3}\] is mixed with \[\ce{CaF2}\] to:

(i) lower the melting point of \[\ce{Al2O3}\].

(ii) increase the conductivity of molten mixture.

(iii) reduce \[\ce{Al^{3+}}\] into \[\ce{Al(s)}\].

(iv) acts as catalyst.


Although carbon and hydrogen are better reducing agents but they are not used to reduce metallic oxides at high temperatures. Why?


In the electrolytic process for the extraction of aluminium the electrolyte is:-


Metal always found in Free State is 


When compared to ΔG° for the formation of Al2O3 ΔG° for the formation of Cr2O3 is


Pyrolusite is ______.


Match List I with List II.

List - I List - II
a. Siderite I. FeCO3
b. Malachite II. CuCO3 · Cu(OH)2
c. Sphalerite III. ZnS
d. Calamine IV. ZnCO3

Choose the correct answer from the option given below.


Match List - I with List - II.

  List - I   List - II
  (One)   (Composition)
(A) Siderite (I) FeCO3
(B) Malachite (II) CuCO3 · Cu(OH)2
(C) Sphalerite (III) ZnS
(D) Calamine (IV) ZnCO3

Choose the correct answer from the options given below:


Calamine and Malachite, respectively, are the ores of ______.


The ore that contains both iron and copper is ______.


Share
Notifications

Englishहिंदीमराठी


      Forgot password?
Use app×