Advertisements
Advertisements
प्रश्न
Indicate the principle behind the method used for the refining of zinc.
Advertisements
उत्तर
Zinc is refined using electrolytic refining process. In this process, pure zinc is transported to cathode from the impure sample at anode. The more basic metal remains in the electrolytic solution and the less basic metals, present as impurities, precipitate as anode mud.
| Electrode | Chemical Reaction |
| Anode | Zn → Zn2+ + 2e- (From anode) |
| Cathode | Zn2+ + 2e- → Zn (From electrolyte) |
APPEARS IN
संबंधित प्रश्न
Write the names and chemical formulae of any one ore of iron.
Describe the roles of the following: SiO2 in the extraction of copper from copper matte
A current liberates 0.50 g of hydrogen in 2 hours. The weight of copper (at. wt. = 63.5) deposited at the same time by the same current through copper sulphate solution is ______.
What happens when a nickel rod is dipped into a copper sulphate solution? Justify your answer.
[\[\ce{E{^{\circ}_{Ni^{+2}/Ni}}}\] = − 0.25 V and \[\ce{E{^{\circ}_{Cu^{+2}/Cu}}}\] = +0.34 V]
When a strip of metallic zinc is placed in an aqueous solution of copper nitrate the blue colour of the solution disappear due to formation of
In the thermite process, the reducing agent is:
Metal always found in Free State is
Native silver metal forms a water solution complex with dilute solution of Na CN in the presence of
Which of the following is not an ore of magnesiuim?
Calamine and Malachite, respectively, are the ores of ______.