प्रश्न
Why does white ZnO (s) becomes yellow upon heating?
Advertisements
उत्तर
The ZnO crystal becomes yellow oh heating because of the metal excess defect which is caused due to the presence of extra cations at the interstitial sites and on heating this white crystal it loses oxygen and turns yellow. The reaction involved is given as-
\[\ce{ZnO ->[heating] Zn^{2+} {+} 1/2 O2 {+} 2e^-}\]
Here the excess of Zn2+ ions move to interstitial sites and electrons to neighbouring interstitial sites.
APPEARS IN
संबंधित प्रश्न
If NaCl is doped with 10−3 mol % of SrCl2, what is the concentration of cation vacancies?
The following diagram shows:

Which of the following will have metal deficiency defect?
Which of the following is a non-stoichiometric defect?
Pink colour of LiCl crystals is due to ______.
Why does table salt, NaCl, sometimes appear yellow in colour?
Match the types of defect given in Column I with the statement given in Column II.
| Column I | Column II |
| (i) Impurity defect | (a) NaCl with anionic sites called F-centres |
| (ii) Metal excess defect | (b) FeO with Fe3+ |
| (iii) Metal deficiency defect | (c) NaCl with Sr2+ and some cationic sites vacant |
A sample of ferrous oxide has actual formula Fe0.93O1.00. In this sample what fraction of metal ions are Fe2+ ions? What type of nonstoichiometric defect is present in this sample?
On doping Ge metal with a little of In (indium), we get:
The non-stoichiometric compound Fe0 940 is formed when x% of Fe2+ ions are replaced by as many `2/3` Fe3+ ions. The value of x is
If NaCl is doped with 10–3 mol % of SrCl2 calculate the concentration of cation vacancies.
Non-stoichiometric defects refer to ______