For the reaction of extraction of \[\ce{Cl2}\] from brine solution:
\[\ce{2Cl^{-} (aq) + 2H2O(l) -> 2OH^{-} (aq) + H2(g) + Cl2(g)}\] the value of ΔGΘ is + ve (442 kJ).
For this value of E– is ΔGΘ = – nFEΘ
or E° = ` - (ΔG^circ)/(nF) = - (422 xx 10^3J)/(2 xx 96500)` = – 2.20 V
Therefore, extraction of \[\ce{Cl2}\] from brine solution will require an external emf more than 2.20 V for electrolysis is process.
APPEARS IN
संबंधित प्रश्न
Name the method of refining of metals such as Germanium.
Explain the principle of the method of electrolytic refining of metals. Give one example.
Explain:
Zone refining
Out of PbS and PbCO3 (ores of lead), which one is concentrated by froth floatation process preferably?
What happens when Silver is leached with NaCN in the presence of air?
What happens when NaCN is added in an ore containing PbS and ZnS during concentration by froth floatation method?
Zone refining is based on the principle that ______.
In which of the following method of purification, metal is converted to its volatile compound which is decomposed to give pure metal?
(i) Heating with stream of carbon monoxide.
(ii) Heating with iodine.
(iii) Liquation.
(iv) Distillation.
Which method is used for refining Zr and Ti? Explain with equation.
How are metals used as semiconductors refined? What is the principle of the method used?
Purification of crude metals by removing metallic and non-metallic impurities is known as ______ of metals.
Refining using liquation method is the most suitable for metals with ______.
Describe a method for refining nickel.
Describe a method for refining nickel.
Describe a method for refining nickel.
Describe a method for refining nickel.
Describe a method for refining nickel.